发布日期:2019-06-27 浏览次数:21
为了不影响环氧地坪整体美观性及正常使用,可以将环氧地坪漆漆膜表面打磨一遍,重新滚一遍面漆。只能将旧漆膜清除干净,重新施工环氧地坪漆。素地需养生28天以上,如有不平或空鼓需加以除去。一旦有不测锋利物体划过的伤口(可以修复,但有微量),应及时修复划痕深,环氧地坪漆底涂层施工前需保持干净如有杂物粘附需清除依照正确比例将主剂及硬化剂混合,充分搅拌。
In order not to affect the overall aesthetics and normal use of epoxy flooring, the surface of epoxy flooring paint film can be polished once and rolled again. Only the old paint film can be cleaned up and the epoxy floor paint can be re-constructed. The vegetable land needs to be kept in good health for more than 28 days. If there is any discrepancy or empty drum, it should be removed. Once there is a wound cut by an unexpected sharp object (can be repaired, but there are trace), deep scratches should be repaired in time. Primer coatings of epoxy floor paint should be kept clean before construction. If there is debris adhesion, the main agent and hardening agent should be removed in accordance with the correct proportion, and fully stirred.
当清洁水或弱碱性洗濯剂,日常的清洁可以用扫帚或软布清洁;使用滚筒或镘刀将材料均匀涂布混合完成材料需30分钟以内施工完成,用中性洗濯剂清洗,运用布洗,然后用清水洗净广州环氧地坪漆,充沛枯燥,打薄的蜡。
When cleaning water or weak alkaline detergent, daily cleaning can be done with broom or soft cloth; using drum or trowel to evenly coat and mix the materials, it takes less than 30 minutes to finish the construction, using neutral detergent to clean, using cloth washing, and then rinsing Guangzhou floor paint with clean water, full and dry, thinning wax.
混合完成材料需30分钟内施工完成;环氧地坪漆不得用硬物,锋利物体间接影响地板,批土养生硬化时间约8小时以上;否则会影响四周的涂层附着力室内焊接和切割施工,将轻巧的设备必需接地罩。